The thin-layer mortar test block has shrunk and has not dried after being left overnight. Is it because the water-reducing agent contains that causes the shrinkage to be so severe?
The dry-mixed mortar sample is fine, but the mass-produced mortar will have a lot of dense bubbles popping up when applied with a trowel. Will this cause a hollow? Have you encountered this situation?
The water consumption is 145, the water retention rate is about 87% (it will still bubble and...
Aerated block masonry mortar formula. Could you guys give me some advice?
Cement 100-120
Coal Ash 50-80
Sand 800-850
HPMC 0.5
Water-reducing agent 1-1.5